ALUMINIUM AW-7075 | AlZn5,5MgCu | AW-AlZn5,5MgCu | AlZnMgCu1,5 | 3.4365 - Fortal

Markings of aluminum and aluminum alloys according to various standards:

Alu/AlloyAW-7075
AA7075
PNPA9
CSN424 222
ASTM USA7075
BS GB7075
BS GP old2L95
ENAlZn5,5MgCu
DIN GERAlZnMgCu1,5
EN7075
ISOAlZn5,5MgCu
JIS JAPANA7075
JIS JAPAN oldA34x6
NF FRANCE7075
NF FRANCE oldA-Z5GU
SFS FINLAND-
SN SWITZAlZn6MgCu1,5
SS SWEDEN-
UNI ITALY9007/2
UNI ITALY old3735
UNSA97075
WNR GERMANY3.4365
NS-
UNEL-3710
ASV2082
ALUSUISSE7215
CSA oldZG62
GOST oldB95V95

Chemical composition of aluminum and aluminum alloys (according to EN 573-1):

Alu/AlloyAW-7075
Mg 2,10 - 2,90 [%]
Mn ≤0,30 [%]
Fe ≤0,50 [%]
Si ≤0,40 [%]
Si+Fe - [%]
Cu 1,20 - 2,00 [%]
Zn 5,10 - 6,10 [%]
Cr 0,18 - 0,28 [%]
Mn+Cr - [%]
Ti ≤0,20 [%]
Bi - [%]
Ni - [%]
Pb - [%]
Sn - [%]
Zr - [%]
Zr+Ti ≤0,25 [%]
Other≤0,05 [%]
different together≤0,15 [%]
Alreszta

Physical Properties of Aluminum:

Alloy - TemperAW-7075 T6
Density2.81 [g/cm3]
E modulus of elasticity72000 [MPa]
Shear modulus G27100 [MPa]
Poissons number0.33
Solidification temperature475 [°C]
Pour point635 [°C]
The right warmth862 [J/kgK]
Coefficient of thermal expansion at 20°C23.5 [µm/mK]
Specific resistance52 [nWm]
Thermal conductivity134 [W/mK]
Conductivity33 [%IACS]

Please send correspondence to the email address below: